| TIDAK | Barang Tes | Satuan | Pertunjukan | Hasil Tes | Metode Tes | ||
| Bahan Belakang | |||||||
| 1 | Kekuatan Tarik | MPa | ≥17 | 19.47 | ASTM D638 | ||
| 2 | Pemanjangan | % | ≥400 | 626 | ASTM D638 | ||
| 3 | Titik Pelunakan Vicat | ºC | ≥90 | 92 | ASTM D1525 | ||
| 4 | Suhu Kerapuhan | ºC | <-65 | <-65 | ASTM D2671C | ||
| 5 | Kekuatan Dielektrik | MV/m | ≥25 | 33.13 | ASTM D149 | ||
| 6 | Resistivitas Volume | Ω.M | ≥1*1013 | 1.1*1013 | ASTM D257 | ||
| 7 | Retak Stres Lingkungan | H | ≥1000 | >1000 | GB/T1842 | ||
| 8 |
Kimia perlawanan (7d) |
10% HCI |
Kekuatan tarik | MPa | ≥85 | 104.9 | ASTM D638 |
| Pemanjangan | % | ≥85 | 96.3 | ASTM D638 | |||
| 10% Tidak |
Kekuatan tarik | MPa | ≥85 | 102.1 | ASTM D638 | ||
| Pemanjangan | % | ≥85 | 95.6 | ASTM D638 | |||
| 10% NaCl |
Kekuatan tarik | MPa | ≥85 | 108.3 | ASTM D638 | ||
| Pemanjangan | % | ≥85 | 94.1 | ASTM D638 | |||
| 9 | Penuaan termal (150ºC,168 jam) |
Kekuatan tarik | MPa | ≥14 | 20.7 | ASTM D638 | |
| Pemanjangan | % | ≥300 | 630 | ASTM D638 | |||
| TIDAK. | Barang Tes | Satuan | Pertunjukan | Hasil Teks | Metode Teks | |
| Perekat | ||||||
| 1 | Titik Pelunakan | ºC | ≥90 | 90.1 | ASTM E28 | |
| 2 | Suhu Kerapuhan | ºC | <-15 | <-15 | ASTM D2671C | |
| 3 | Geser Putaran | MPa | ≥1.0 | 1.5 | ASTM D1002 | |
| 4 |
Kekuatan Kupas (23±2ºC) |
Baja | N/cm | ≥70 | 145.6 | ASTM D1000 |
| Dasar | N/cm | ≥70 | 205.9 | ASTM D1000 | ||
| lapisan PE | N/cm | ≥70 | 190.0 | ASTM D1000 | ||
| Primer Epoksi non-pelarut | ||||||
| 5 | Geser primer yang sudah diawetkan | MPa | ≥5.0 | 12 | SY/T0041 | |